Suppose a receiving team checks a batch of moulded impellers. The caliper reading agrees with the diameter drawing, but a trial assembly rubs. A thin lip is visible where the parting line crosses a vane tip near the cover. The whole impeller need not be too large. Local flash can sit between the usual measurement contacts or project axially toward the cover. Look at the space the vane actually sweeps and the clearance to the mating part. Keep photographs before anyone trims the evidence.
Diameter and a local protrusion describe different things
Melt can escape where the mould closes and leave a thin edge after cooling. A gate vestige comes from the place where the plastic enters the cavity, which can leave a different mark in a different location. Colour or touch alone cannot identify the manufacturing cause. Compare the part with known parting and gate locations and a good sample from the cavity. Establish how far the material sticks out, in what direction and whether it enters a working surface.
A two-point diameter check can miss a protrusion on just one vane. A very thin lip can also deflect against the measuring jaws and spring back. A feature sticking toward the cover of an open or semi-open impeller affects axial clearance without necessarily changing the measured outside diameter. Radial protrusions matter where the impeller passes close to the chamber wall. Marks can also come from impeller runout, bearing play, installed depth or cover geometry. A circular rubbing mark alone does not establish flash as the cause.
Mark the areas that matter on the incoming plan
Before assembly, identify the vane tips, cover-facing face and surfaces close to the chamber wall. Agree on lighting, magnification and a way to measure any protrusion. Pay attention where the mould parting line crosses these areas. Sample each cavity as applicable and record the tool and lot identity. If the drawing only states diameter, ask engineering to define the allowable protrusion in the functional areas, acceptance samples and a suitable method before making that an independent rejection criterion. Material that can detach also deserves an assessment of where it might go.
When checking contact, retain the impeller and cover marks and compare them with installed depth and axial location. Check whether damage corresponds to a feature on an individual vane. With power isolated, authorised service or test personnel can use the approved fixture to check freedom of movement. Any powered test belongs in a correctly reassembled unit within its permitted conditions. Do not run the pump to wear away flash or have receiving staff trim each part until it stops rubbing. Production rework can remove functional material and should require approval and reinspection.
Actual room for a protrusion can be much less than nominal clearance
For illustration, suppose nominal axial clearance is 0.30 millimetres. The tightest position in one assembled example has 0.15 millimetres of remaining room after the parts and runout are considered. A local lip extending 0.20 millimetres toward the cover could touch there even if the radial diameter passes. This is an example of checking the right direction, not a recommended tolerance. If a known sound impeller also rubs at the same place, check the cover and shaft before blaming more parts.
For a repeat order, retain accepted cavity samples and photographs. Use the agreed sampling process to narrow the affected cavity or time window and hold the relevant stock. After tooling work or approved trimming, confirm samples under the same measurement arrangement and check the mating assembly. A buyer should know which vane and surface interfere, not simply receive another report that the overall diameter passed.
Frequently asked questions
Will any flash make an impeller rub?
No. Its position, direction, clearance and the mating parts determine whether it can interfere. Use the drawing and agreed risk assessment elsewhere.
Is every visible parting line a reject?
No. A visible seam is different from excess material standing proud. Judge the protrusion against the approved method and sample.
What has to be checked after approved trimming?
Recheck the required dimensions, local shape, any loose material and assembly clearance. Do not let the absence of audible rubbing stand in for inspection.